What kind of brazing rod do I need for aluminum?
Super Alloy 5 can be applied with any heat source (we recommend oxyacetylene or oxy-MAPP for brazing large aluminum pieces or thick aluminum parts such as aluminum boats) at a very low temperature: 600°F, half the melting temperature of pure aluminum.
How strong is aluminum brazing rod?
33,000 psi
With a low working temperature of 720 to 750 degrees Fahrenheit, these rods can also be used to build up aluminum joints without distortion, discoloration or loss of strength. They have a tensile strength of 33,000 psi.
Should you use flux when brazing aluminum?
Aluminum braze flux is required in all aluminum brazing operations. Aluminum brazing fluxes consist of various combinations of fluorides and chlorides and are supplied as a dry powder. For torch and furnace brazing, the flux is mixed with water to make paste.
How do you seal cracks in cast aluminum?
Instead, use a carbide cutter or a cutting wheel to “V” the crack on the outside out to provide a place for the filler metal to be deposited. Then weld the outside, turn the casting over, and do the same to the inside surface. With this method you have a good chance to deposit a strong, leak-free weld.
Can you braze aluminum with MAPP gas?
It is an easy way to weld aluminum, with no flux or shielding gas, and only requires an inexpensive tank of propane or MAPP gas, easily purchased at your local hardware store. Then again, there is always JB Weld for those down and dirty connections.
What is stronger welding brazing or soldering?
Brazing being stronger than soldering, but there are no effects on the base material in soldering. The lowest temperature used for soldering and brazing. Brazing needs filler flux along the high temperature to join the parts.
Is JB Weld good on aluminum?
For a reliable aluminum epoxy that can handle medium- to heavy-duty jobs, the J-B Weld KwikWeld epoxy has a 5,020 PSI rating and withstands temperatures of over 500 degrees Fahrenheit, making it an ideal option for cars, RVs, and boats.
Will hts-2000 work on aluminum?
HTS-2000 will successfully join all aluminum alloys, including those that are not favorably joined by high-temperature brazing. When drawn over heated aluminum, HTS-2000 penetrates the aluminum oxide, creating a molecular bond that is stronger than the original commercial aluminum.
What is hts-2000 brazing rod?
Made for all non-ferrous metals and aluminum parts, HTS-2000 is a second generation Industrial Strength Brazing Rod created from a revolutionary new formula. Not to be confused with Alumaloy, Alumaweld, Alumarod, Durafix, Aladdin 3 in 1, or any other first generation rods most of them consisting of 3 alloys.
How much is a pound of hts-2000?
HTS-2000 has been sold in more than 40,000 professional shops at $100.00 a pound, with a minimum order of 5 pounds. On the Internet only, you may order a 1 lb. HTS-2000 STARTER PACKAGE! Plus for a limited time we’ve slashed the price by as much as 50 percent! Choose the right amount for you, order securely online, and SAVE a bundle!
What is the difference between the first generation rods and hts-2000?
HTS-2000 has an elongation of 10% in 2 inches (rather than the standard 3% like the first generation rods listed above) which makes HTS-2000 3 times more flexible and stronger than any of its competitors. It also easily penetrates past impurities that lay below the metal’s surface which may be impossible to penetrate with competitors materials.